Home » Products » PV Encapsulation Materials » PV Functional Film » HI803 HJT Integrated Encapsulation Film
HI803 HJT Integrated Encapsulation Film
- HI803 is also designed for high-reliability HJT module encapsulation, helping protect solar cells in damp-heat environments and reducing the risk of hot spots, delamination, and corrosion.
- With >75% crosslinking degree, PCT yellowness index below 3.0, and UV aging ΔYI below 3.0, HI803 is ideal for heterojunction modules requiring long-term stability, aging resistance, and reliable encapsulation.
Get a Free Consultation
Get a Free Consultation
| Product Specifications | ||
| Specifications | Normal Specifications | Customized Specifications |
| Thickness | 0.45mm – 0.6mm | 0.2 – 0.8mm |
| Width | 970 – 1297mm | 300 – 1300mm |
| Length | 300m | 150 – 450m |
| Technical Properties | |||
| Item | Test Standard | HI803 | |
| Using Instruction | High Transmittance | ||
| Shrinkage Ratio | MD | GB/T29848 | <3.0% |
| TD | GB/T29848 | <5.0% | |
| Light Transmittance | 280 – 380nm | Betterial | >80% |
| 380 – 1100nm | GB/T29848 | >90% | |
| Peel Strength | Glass | GB/T29848 | >80N/cm |
| Solar Cell | Betterial | >40N/cm | |
| Crosslinking Degree | GB/T29848 | >75% | |
| Volume Resistivity | GB/T29848 | >1*10^15 Ω·cm | |
| Damp Heat Test | Yellowness Index (YI) (PCT 48h 121℃ 100RH ) | GB/T 29848-2018 | <3.0ΔYI |
| Solar Cell (PCT 48h 121℃ 100RH ) | Betterial | >30N/cm | |
| UV Test(UV 30kW/h 60℃) | GB/T 29848-2018 | <3.0ΔYI | |
| Laminating Process | ||||
| Laminated Parameters | Temperature(℃) | Vacuum Time(S) | Lamination Time(S) | |
| Single Chamber Laminator | 142 – 148 | 300 – 360 | 900±180 | |
| Double Chamber Laminator | Cavity 1 | 120±10 | 300±60 | 300±60 |
| Cavity 2 | 148±10 | 60±30 | 540±60 | |